In the industry that I work in they have always used shrouded impellers and I am now wondering why. Looking at the alternative and not using a shroud I see a a possibility of easy maching (CNC with great surface finishes), no efficiency loss from wear ring clearance, and less material so lower weight. Using the shroud we have to cast the impellers which is not accurate and we can not thoroughly check them and the surfaces are horrible. Does anyone know why we should not being using shroudless impellers.
The industry is multistage pumps for the LNG gas industry. (methane, propane, butane)
The industry is multistage pumps for the LNG gas industry. (methane, propane, butane)