Are the dimensional changes are due to loss of absorbed water or due to stress relieving?

Thanks in advance for the response.


 
Replies continue below

Recommended for you

With PPS it will be because of stress relieving or maybe increased crystallinity. Almost certainly stress relieving.

Regards
Pat
See FAQ731-376 for tips on use of eng-tips by professional engineers &
for site rules
 
You can check which by DSC. Increased crystallinity is easily detectable.

Relief of stresses is too under polarized light.