I want to know the temperature for shrinkage fitting. i want to fit a ring of outer dia 715mm, inside dia 675mm into hole of dia 684, then upto how much temperature i have to cool ring to fit into the hole ?
 
Replies continue below

Recommended for you

Do you know the material of which the ring, and the hole, are made?

WE DON'T.


Mike Halloran
Pembroke Pines, FL, USA
 
Cast iron has a coefficient of thermal expansion of around 10.5x10-6 m/m/K

To fit a 715 diameter ring into a 684 diameter hole, you need a shrinkage strain of about 4.3%.

This would need a temperature drop of around 4000 K (or a temperature rise in the hole of around the same amount, assuming it is also cast iron).

Are you sure your parameters are correct?

Student question?

 