Hello all,
We have had some discussions with suppliers whether or not the ASTM codes should be stated on the certificates.
For instance when we order material per ASTM A182 F316L.
ASTM A182 par 16 refers to ASTM A961.
ASTM A961 par 19.2 reads: "...They shall contain the information specified by the Product Specification and the purchase order. They shall include the specification number and year/date of issue"
Or we order for instace material per ASTM A240 type 316L.
ASTM A240 par 3 refers to ASTM A480.
ASTM A480 par 8.1 reads: "A report of the results of all tests required by the product specification shall be supplied to the purchaser. This material test report shall reference to the specification designation and year date indicating that the material was manufactured, sampled, tested, and inspected in accordance with requirements of the product specification and has been found to meet those requirements..."
Should our supplier mention the ASTM code on the certificates?
Thanks
Kitty
We have had some discussions with suppliers whether or not the ASTM codes should be stated on the certificates.
For instance when we order material per ASTM A182 F316L.
ASTM A182 par 16 refers to ASTM A961.
ASTM A961 par 19.2 reads: "...They shall contain the information specified by the Product Specification and the purchase order. They shall include the specification number and year/date of issue"
Or we order for instace material per ASTM A240 type 316L.
ASTM A240 par 3 refers to ASTM A480.
ASTM A480 par 8.1 reads: "A report of the results of all tests required by the product specification shall be supplied to the purchaser. This material test report shall reference to the specification designation and year date indicating that the material was manufactured, sampled, tested, and inspected in accordance with requirements of the product specification and has been found to meet those requirements..."
Should our supplier mention the ASTM code on the certificates?
Thanks
Kitty