hi, all friends.
it is me problem...
vanes of blast and blindage with more replace...
I need alternative for it...
help me, please.
 
Laser shock peening is an alternative surface treatment. High intensity laser pulses are used to develop deep compressive residual stresses in the component surface, many times deeper than metal shop peening.

I believe TurboCare offers this service.



Dave G.
 