Hi,

Our customer has a 6063-T6 aluminum pipe specification for the resin pellet transport asking that all pipe, elbow, etc. shall be shot peened inside (hammer finish). What are the advantages to do this kind of treatment? Also, what is the differences between mechanical or chemical to realize this finish?

Regards,

Hcjulien
 
This is for errosion protection. A number of Owner's require this for systems transporting plastic pellets.

 
Thank stanweld,

is it done chemically or mechanically?

Regards,

hcjulien
 