Mar 15, 2012 #1 irq Aerospace Joined Jan 18, 2008 Messages 45 Location AT I have the stress strain data of the rubber tested in compression. Do anybody know how I can obtain from these data Shore A of the material? Thanks!
I have the stress strain data of the rubber tested in compression. Do anybody know how I can obtain from these data Shore A of the material? Thanks!
Mar 16, 2012 #2 tom1953 Chemical Joined Jul 25, 2005 Messages 177 Location US I have never hear that there is a correlation between stress/strain data and hardness. tom Upvote 0 Downvote
Mar 16, 2012 #3 GrahamBennett Materials Joined Feb 1, 2007 Messages 1,308 Location GB As far as I know there is no correlation between hardness and stress/strain data. Upvote 0 Downvote
Apr 12, 2012 #4 mcclain Mechanical Joined Apr 24, 2003 Messages 39 Gent, Engineering with Rubber, indicates an empirical relationship between Shore hardness and initial Young's modulus. Upvote 0 Downvote
Gent, Engineering with Rubber, indicates an empirical relationship between Shore hardness and initial Young's modulus.