Our typical shop preperation for a beam to beam moment weld is to bevel the flanges 30 degrees (60 degree total angle), cut the web on each member with a 1"x1" "APPLE", use a back up bar and weld it complete.
Can a moment connection be achieved the same way with a C12X20.7 to C12X20.7? The problem I am having is the graduated thickness of the channel flange. Will the weld thickness graduate 3/8" to 5/8"?
Can a moment connection be achieved the same way with a C12X20.7 to C12X20.7? The problem I am having is the graduated thickness of the channel flange. Will the weld thickness graduate 3/8" to 5/8"?