Dear members
According to attached drawing,the manufacturer has recommended shell test pressure=78bar.
in the other hand since the material is A494-N12MV then shell test pressure would be
1.5*41.4=62.1 bar
(41.4=working pressure @38c as per ASME B16.34)
So how can it be justified?
regards
Arash
According to attached drawing,the manufacturer has recommended shell test pressure=78bar.
in the other hand since the material is A494-N12MV then shell test pressure would be
1.5*41.4=62.1 bar
(41.4=working pressure @38c as per ASME B16.34)
So how can it be justified?
regards
Arash