Can anyone direct me to suppliers in the US who can make rolled shells about 24" to 60" in diameter and length from 10' to 24' made of carbon steel and stainless steel.
Thanks.
 
haggis, thanks for the link.
 
asv80,

One source that can make rolls (consisting of single or multiple wall/shells) is Morrison-Berkshire, in North Adams, MA. They roll their own components, and can turn a 6' X 60' roll.

They can roll 1/2 or even thicker material, up to 20' long.

BK
 
bk:
thanks for the information.
 