Shell forming method with low out of roundness for thin shell

BasakAbhishek

Mechanical
Joined
Sep 5, 2006
Messages
41
Location
IN
Hello,
My job requires forming a shell of Inconel625 of 2m ID, 6mm thickness, 2m long. The permissible out of roundness is 0.25%. Any idea how this can be achieved? Is there any other method other than a pyramid roller (maybe like forming on a carbon steel "mandrel"?
Thanks
Abhishek
 
OP
Contact a custom tube and pipe shop.
If they have the correct facilities.
It can be slip rolled, welded , weld planished
Annealed, then pulled thru a draw die to obtain diameter size. However because it is thin wall and that size. Diameter roundness will be in the constrained condition.
 
mfgengear
I mentioned the dimensions, 2m ID, 6mm thk, 2m long..its obviously not a pipe and cannot be drawn though a die...
 
mfgengear
I mentioned the dimensions, 2m ID, 6mm thk, 2m long..its obviously not a pipe and cannot be drawn though a die...
how do you know, then if you know why are you asking.
take your drawing to a shop , and not just one , several until you find the right one.
I said a tube and pipe shop. that can handle that size. it's going to a specialty shop that knows how to make precision tube and pipe of any size.
 
if a tube and pipe shop can handle 2m dia shells of Inconel 625 and can draw them through a die then it must be the best in business with huge presses and thousands of square metres in floor space...and if I could have taken the drawing to a shop, then is there any need for posting the question on eng-tips, is it?
 
if a tube and pipe shop can handle 2m dia shells of Inconel 625 and can draw them through a die then it must be the best in business with huge presses and thousands of square metres in floor space...and if I could have taken the drawing to a shop, then is there any need for posting the question on eng-tips, is it?
I not doing your job for you it's obvious your over your head and been insulant isn't helping.
You don't have the expertise or equipment to handle it
Thin was wall large diameter is pita. You would scrap it out. And get fired. Good luck
 
if I knew what to do..would I have come to this forum?..... and no "go to a shop" is not helpful at all
 
It takes special fabricated draw die. The part needs excess swaged down slightly.
A draw ram with a special clamping mandrel
That clamps the end of the part. That end will be trimed later. To net size.
Dies are expensive. There has to be a draw bar ram , hydraulic
Option would be to expand the ring in a press with a rubber inside the ring. It would require to
Develope size. All very expensive equipment and investment. Op you could do the first part and the farm out the expansion or draw.
 
Form, weld, and roll.
No one can draw this size.
There are forges but they are suitable for such thin walls.
Lol ED I been know to do the impossible. That was my job. Build the unbildable. Being do it all my life. Thats why I got old.
 
What it becomes is how much money one wants to spend. And what they can really live with.
Stations on large aircraft and large missiles where held to ÷/_ ,001 length.
There was comment once said
Don't tell me the odds.

.
 
A hefty log, heavy wooden hammer and a several strong man with skill and patience.
 
No problem. First the heads must be at the manufacturer prior to rolling the shell.
 
No problem. First the heads must be at the manufacturer prior to rolling the shell.
Why?
Can't two shops in the US work to/achieve the same tolerance?
 
How do you plan to make a cylindrical shell that fits perfectly with the head if you don't have the head yet?
 