Hello

I need to determine the 3003 H-14 aluminum equivalent of 304 stainless steel. For instance, I have a .125" thick 304 S/S sheet metal part. I need to determine the thickness of the aluminum sheet metal that will have the same strength as the existing stainless steel part. It's been a while since I've done this and I'm lost. Can anybody please help me get started? Thanks!

 
Lots of unknowns and nowhere to start.

Need to have some idea of the application, geometry, loading, etc.

<tg>
 
Just assume 200lbs of tensile strength. Also assume the sheet is being hung vertically with the top mounted and the bottom supporting the load.
 
If this is a structural bracket you might want to think about 2024-T3 instead of 3003-H14.

Can you post a picture of the bracket installed in its intended use. Is this bracket mounted in an enclosure or a vehicle (plane, or truck)

Heckler
Sr. Mechanical Engineer
SWx 2007 SP 2.0 & Pro/E 2001
XP Pro SP2.0 P4 3.6 GHz, 1GB RAM
NVIDIA Quadro FX 1400
o
_`\(,_
(_)/ (_)

(In reference to David Beckham) "He can't kick with his left foot, he can't tackle, he can't head the ball and he doesn't score many goals. Apart from that, he's all right." -- George Best
 
Annealed 304 stainless steel has a yield strength of approximately 200 MPa.

3003-H14 aluminium has a yield strength of 145 MPa.

If your Al part needs to have equivalent strength to 3 mm thick 304 stainless steel, then the thickness would need to be t =(200 MPa/145 MPa)[&middot;] 3 mm = 4 mm.

Regards,

Cory

Please see FAQ731-376 for tips on how to make the best use of Eng-Tips Fora.
 
Thanks guys.

Cory, I double checked my calcs according to your suggestion and it seems I was doing it correctly. Thanks again.
 
Since your application is simple tension it can be approached this way. A complex beam or shear application could yield different results. Also, your definition of same strength might impact the results.

Think about a rubberband and a string. If you incrementally add weights hanging from a string and rubberband and they both break at the same weight, does that mean they were the same strength? Not if your concern was you wanted a small deflection from the rubberband, similar to the string. Then you'd need alot thicker rubberband...