M
MatthewJB19904
Guest
Have anyone had any luck trying to drive the sheet metal parameters with relations? For instance - SMT_DFLT_BEND_RADIUS is a standard parameter in the list. I want to drive that parameter with a relation of table. Since the pulldown shows "thickness","thickness*2" & "by parameter". Since each material type and thickness comes with its own inside bend radius is it possible to drive this parameter with a relation... perhaps just a IF statement.
EX - IF MATERIAL=="18/4"
SMT_DFLT_BEND_RADIUS=.03
(and so on for other materials)
This way I don't have to key it in when making walls. Its calculated the same way a bend table calculates the developed length.
I have not been successful yet. Anyone have any ideas?
Matthew
EX - IF MATERIAL=="18/4"
SMT_DFLT_BEND_RADIUS=.03
(and so on for other materials)
This way I don't have to key it in when making walls. Its calculated the same way a bend table calculates the developed length.
I have not been successful yet. Anyone have any ideas?
Matthew