Jun 27, 2018 #1 alarson Mechanical Joined Jun 13, 2018 Messages 6 Location US Hi all, I'm trying to coin a region down to ~70% thickness and then bend across that region. Is there a way to do that while maintaining the sheet metal feature? An example part is attached. Thanks! https://files.engineering.com/getfile.aspx?folder=763fa1ca-7a51-4884-bde5-803b51c8787e&file=Coined_Hinge.SLDPRT
Hi all, I'm trying to coin a region down to ~70% thickness and then bend across that region. Is there a way to do that while maintaining the sheet metal feature? An example part is attached. Thanks!
Jun 27, 2018 Thread starter #2 alarson Mechanical Joined Jun 13, 2018 Messages 6 Location US I got this one answered over on the SW forums. https://forum.solidworks.com/thread/221560 Upvote 0 Downvote
Jun 28, 2018 1 #3 SBaugh Mechanical Joined Mar 6, 2001 Messages 6,691 Location US Yeah, he is correct, because SW requires sheet metal to be a uniform thickness. Scott Baugh, CSWP CAD Systems Manager Evapar http://www.evapar.com "If it's not broke, Don't fix it!" Click to expand... faq731-376 Upvote 0 Downvote
Yeah, he is correct, because SW requires sheet metal to be a uniform thickness. Scott Baugh, CSWP CAD Systems Manager Evapar http://www.evapar.com "If it's not broke, Don't fix it!" Click to expand... faq731-376