In an existing brick wall of some 14 inches thick minimum,
is there a rational guide to determine the probable shear capacity of the mortar present? Is there a small compression test that can be applied to the mortar in place?
This is in an urban environment that probably had reasonably up to date practice as established at that time. So can information be developed that would be satisfactory to a Building Department?
is there a rational guide to determine the probable shear capacity of the mortar present? Is there a small compression test that can be applied to the mortar in place?