Due to a design error a shaft supporting a horizontal rotor has failed. The manufacturer has agreed that the failure is due to a design fault and is replacing the shaft. The manufacturer has provided design calculations, which appear to be ok, but I need to check the various factors and formulae that have been used.
Can anyone recommend a good text book that will provide the detailed background and the tables of factor needed to establish the design stress.
The shaft torque is 3880 Nm and the bending moment is 878 Nm.
The shaft size 80 mm, increasing to 100 mm.
The proposed marterial is 42CrMo4.
Can anyone recommend a good text book that will provide the detailed background and the tables of factor needed to establish the design stress.
The shaft torque is 3880 Nm and the bending moment is 878 Nm.
The shaft size 80 mm, increasing to 100 mm.
The proposed marterial is 42CrMo4.