ridwansunarya
Chemical
Dear All,
I'm new here, i've got a problem with this stuff. Anyone care to look at this failed shaft?
It was a centrifugal pump with double suction enclosed type impeller and shaft supported with plane bearing on both ends
I'd like to know if it is torsion or fatigue or even something else that might cause it to break like this?
Material : A276 316L
Fluids service : MDEA Semi-Lean Solution
RPM : 2980
Suction Pressure (Max/Rate) : 9.0/3.8 kg/cm2G
Discharge Pressure : 36.4 kg/cm2G
Thanks !
I'm new here, i've got a problem with this stuff. Anyone care to look at this failed shaft?
It was a centrifugal pump with double suction enclosed type impeller and shaft supported with plane bearing on both ends
I'd like to know if it is torsion or fatigue or even something else that might cause it to break like this?
Material : A276 316L
Fluids service : MDEA Semi-Lean Solution
RPM : 2980
Suction Pressure (Max/Rate) : 9.0/3.8 kg/cm2G
Discharge Pressure : 36.4 kg/cm2G
Thanks !