What causes rivets to bend off-axis rather than crushing straight down along the long axis of the rivet when you try to set them?
I am setting some 5/32 aluminum rivets (AN470AD-5-8)to fasten a patch piece onto the hull of my boat. If I use a long enough rivet to give 1/4" protrusion they don't always set right. Some try to bend over rather than crush straight down. Going to a 1/8" shorter rivet solves the problem, but now the rivet head isn't thick enough (I think).
I've got a rivet gun with the appropriate rivet set. I can't blame the person on the buck bar because my wife is helping me.
The hull is thickness is 0.100 and the patch piece is 0.125. The rivet length is 0.50, leaving a 0.275 stub poking through the hull of the boat to set the buck bar on.
I drilled the holes through the patch piece on a drill press, so they are square. I drilled the holes through the hull by hand, so some aren't perfectly sqaure to plane of the hull.
So far as I can tell, a 5/32 rivet should be ~0.25 longer than the grip to get a good head. Mine are ~0.275 longer.
Some set up perfect, but many lean over.
What am I doing wrong? Thanks
I am setting some 5/32 aluminum rivets (AN470AD-5-8)to fasten a patch piece onto the hull of my boat. If I use a long enough rivet to give 1/4" protrusion they don't always set right. Some try to bend over rather than crush straight down. Going to a 1/8" shorter rivet solves the problem, but now the rivet head isn't thick enough (I think).
I've got a rivet gun with the appropriate rivet set. I can't blame the person on the buck bar because my wife is helping me.
The hull is thickness is 0.100 and the patch piece is 0.125. The rivet length is 0.50, leaving a 0.275 stub poking through the hull of the boat to set the buck bar on.
I drilled the holes through the patch piece on a drill press, so they are square. I drilled the holes through the hull by hand, so some aren't perfectly sqaure to plane of the hull.
So far as I can tell, a 5/32 rivet should be ~0.25 longer than the grip to get a good head. Mine are ~0.275 longer.
Some set up perfect, but many lean over.
What am I doing wrong? Thanks