Service Index - Materials Compatibility

Status
Not open for further replies.

Huber

Mechanical
Joined
Feb 7, 2001
Messages
2
Location
US
I am searching for a fairly comprehensive service index with compatibility information on various fluids vs. common alloys used in piping systems. Any help would be appreciated.
 
The most complete corrosion and chemical compatibility guide that I am aware of is the Compass guide. I believe they have a website. The guide is available on CD and covers alloys as well as plastics.
 