I am searching for a fairly comprehensive service index with compatibility information on various fluids vs. common alloys used in piping systems. Any help would be greatly appreciated.
 
Hi Huber,

You can start with Perry Table 28-2 (p 28-30 ),General Corrosion Properties of Some Metals and Alloys..

Manufacturers such as Cabot..etc have comparison tables.
Also check(
Good luck

Whylie
 