Dear colleagues
We are a looking for separable coating material (identical to Foamfrax material) for the external parts of power plant turbine for thermal and and insulation reason.


 
Help! Does any one know about such product?
 
I don't know where you are located, but you might try insulating blankets. Follow the link below for Pacor, an insulation fabriator, located in the state of New Jersey in the USA:


Just a note of caution - the blankets must be held closely to the turbine casing, especially on the lower half. Blankets are usually held in place by stainless steel wire threaded through eyelets (or Nelson studs) welded to the turbine casing.

You will need to find a local insulation contractor to take measurements for fabrication of the blankets.

Best of luck!
 
Unfortunately BNZ do not carry coating material, just bricks and panels. If you have any other idea how carry separable coating material it will be very helpful.
Happy New Year

 