Nov 9, 2008 #1 FC2008 Mechanical Joined Aug 4, 2008 Messages 106 Location GB Hi, what are semi finished bolts? I've done a google search with no luck. Thank you
Nov 9, 2008 #2 gr2vessels Mechanical Joined Sep 29, 2004 Messages 1,971 Location AU The unfinished thread is one example. Another is missing the hex head, I have seen recently a pack of Chinese bolts with Phillips head, missing the cross slots. No refund given... cheers, gr2vessels Upvote 0 Downvote
The unfinished thread is one example. Another is missing the hex head, I have seen recently a pack of Chinese bolts with Phillips head, missing the cross slots. No refund given... cheers, gr2vessels
Nov 9, 2008 Thread starter #3 FC2008 Mechanical Joined Aug 4, 2008 Messages 106 Location GB I have a drawing with this specification: Stud Bolt, 1 1/8'' x 230mm, A193-B7 w/2 A194-2H Nuts, Semi-Finished. Does this mean that the nuts are not done? Confusing. Thank you. Upvote 0 Downvote
I have a drawing with this specification: Stud Bolt, 1 1/8'' x 230mm, A193-B7 w/2 A194-2H Nuts, Semi-Finished. Does this mean that the nuts are not done? Confusing. Thank you.
Nov 10, 2008 #4 hydtools Mechanical Joined Apr 4, 2007 Messages 3,265 Location US Semi-finished nuts are tapped and one face finished flat, perpendicular to the thread. From American Machinists' Handbook. Ted Upvote 0 Downvote
Semi-finished nuts are tapped and one face finished flat, perpendicular to the thread. From American Machinists' Handbook. Ted