Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Semi finished bolts

Status
Not open for further replies.

FC2008

Mechanical
Aug 4, 2008
106
Hi,
what are semi finished bolts?
I've done a google search with no luck.

Thank you
 
Replies continue below

Recommended for you

The unfinished thread is one example. Another is missing the hex head, I have seen recently a pack of Chinese bolts with Phillips head, missing the cross slots. No refund given...
cheers,
gr2vessels
 
I have a drawing with this specification:

Stud Bolt, 1 1/8'' x 230mm, A193-B7 w/2
A194-2H Nuts, Semi-Finished.

Does this mean that the nuts are not done? Confusing.

Thank you.
 
Semi-finished nuts are tapped and one face finished flat, perpendicular to the thread. From American Machinists' Handbook.