Hello & Good Evening
Selection of IQI as per ASME Sec.V
With reference to ASME Sec.V Article 2, Cl.T-276.2(a) For Welds with reinforcements, the thickness on which IQI is selected is nominal Single Wall Thickness plus estimated weld reinforcement, Backing strips or rings shall not be considered as a part of thickness.
My question is that While considering the Weld reinforcement whether we have to consider both external reinforcement and internal root penetration for Selection of IQI or only we have to consider External reinforcement.
Thanks
Selection of IQI as per ASME Sec.V
With reference to ASME Sec.V Article 2, Cl.T-276.2(a) For Welds with reinforcements, the thickness on which IQI is selected is nominal Single Wall Thickness plus estimated weld reinforcement, Backing strips or rings shall not be considered as a part of thickness.
My question is that While considering the Weld reinforcement whether we have to consider both external reinforcement and internal root penetration for Selection of IQI or only we have to consider External reinforcement.