The client was asking recommendations on durable painting system to be applied to the exterior surfaces of large (20' diameter), tall (150') steel (base material unclear) stacks located in a steel mill setting (sinter plant) at the midwest region, close to lake. The paint selected should be able to sustain 400 degrees of heat and chemical attack from furnace gas. Any suggestion on the paint material/spec/standard/vendors is appreciated. Thanks in advance.
 