Seek recommendations for braze fixturing materials
Brazing carbide at up to 1500 F
1. High strength rods to position parts during brazing
2. Somewhere the previous person found 2 materials
A. a material that looks sort of like a particle board
B. a material that looks like has mica in it with a green layer on one side
I would appreciate any recommendations anyone cares to make.
Thanks,
Tom
Thomas J. Walz
Carbide Processors, Inc.
Good engineering starts with a Grainger Catalog.
Brazing carbide at up to 1500 F
1. High strength rods to position parts during brazing
2. Somewhere the previous person found 2 materials
A. a material that looks sort of like a particle board
B. a material that looks like has mica in it with a green layer on one side
I would appreciate any recommendations anyone cares to make.
Thanks,
Tom
Thomas J. Walz
Carbide Processors, Inc.
Good engineering starts with a Grainger Catalog.