Hello all-
We have a necked style flange welded to the spherical head of a pressure vessel (design pressure 1000psi). The pressure vessel is not a code stamped item and is unique to a test site, but we are treating it as a Section VIII Div 1 code vessel anyway.
The flange is an ASTM A105 forging and the spherical head is forged as well. The weld joint is a full penetration weld of the type shown in Section VIII Fig UW-16.1(d), and does not have a separate reinforcement plate. I presume this type of weld means it is NOT a category D butt weld as depicted in Figure UW-3.
The weld requires either a full depth repair of a crack which developed while in service, or we may elect to remove the flange and reweld a new flange with the entire full penetration circumferential weld, same as before.
By Section VII Div 1 requirements, does this weld require RT if it is either repaired or completely removed and rewelded? I cannot find the code citation which will help me to determine this, Please help.
Other info: The flange is 10-inches at it’s O.D and has a 3.83-inch diameter bore. There is about 2 ¼-inch distance between the underside of the flange and the spherical head. (RT, if required would be indeed difficult).
Thanks for any help on this question.
Tom
We have a necked style flange welded to the spherical head of a pressure vessel (design pressure 1000psi). The pressure vessel is not a code stamped item and is unique to a test site, but we are treating it as a Section VIII Div 1 code vessel anyway.
The flange is an ASTM A105 forging and the spherical head is forged as well. The weld joint is a full penetration weld of the type shown in Section VIII Fig UW-16.1(d), and does not have a separate reinforcement plate. I presume this type of weld means it is NOT a category D butt weld as depicted in Figure UW-3.
The weld requires either a full depth repair of a crack which developed while in service, or we may elect to remove the flange and reweld a new flange with the entire full penetration circumferential weld, same as before.
By Section VII Div 1 requirements, does this weld require RT if it is either repaired or completely removed and rewelded? I cannot find the code citation which will help me to determine this, Please help.
Other info: The flange is 10-inches at it’s O.D and has a 3.83-inch diameter bore. There is about 2 ¼-inch distance between the underside of the flange and the spherical head. (RT, if required would be indeed difficult).
Thanks for any help on this question.