There is a company that is considering the use of 4" PEAD piping in captation gas the questions are the following:
1.-What could be the effect in a steel pipe make a change in a section (of about 500 to 1200meters) using PEAD (type PE100)
2.-The fluid is wet gas ( we called it to hidrocarburo in liquid state for example gasoline, condensed) with very high presence of sulphydric acid (H2S) (400-500ppm) at a max pressure of 4 bar.
3.- What could be the effect to make a section change reducing from 10 to 4"
Thanks in advance for yours attention.
Patrick
There is a company that is considering the use of 4" PEAD piping in captation gas the questions are the following:
1.-What could be the effect in a steel pipe make a change in a section (of about 500 to 1200meters) using PEAD (type PE100)
2.-The fluid is wet gas ( we called it to hidrocarburo in liquid state for example gasoline, condensed) with very high presence of sulphydric acid (H2S) (400-500ppm) at a max pressure of 4 bar.
3.- What could be the effect to make a section change reducing from 10 to 4"
Thanks in advance for yours attention.