Regarding Table QW-416 Filler Metals QW-404.23 Solid or metal-cored to flux cored: in the Brief of Variables column, the Legend symbol is "t" indicating thickness. Is that symbol correct or should the "Change" symbol have been used??
 
Replies continue below

Recommended for you

Yes, it appears so. I compared the 2004 Edition (Article IV Welding Data) with the 2003 Addendum (Article IV), and the 2003 Addendum shows no symbol at all for filler metal QW-404.23 in Table QW-416.

Interestingly, if you review the essential variables for the welding processes in QW-255, they show a change symbol for QW-404.23.
 

There is no symbol for this essential variable (Gtaw &Paw),
pl refer QW 256
 