I've been looking at small (something like 18650 size) lithium-ion batteries for a portable application. However, these batteries typically don't want to be charged above a temperature of 45C or discharged above 60C. Does anyone know of a source of other types of batteries that can safely tolerate somewhat higher temperatures (maybe charging around 55-60C and discharging at 70-75C)?
Thanks in advance,
Glenn
Thanks in advance,