Hi,
how much seating force required to control leakage for following requirements.
Allowable leakage when closed condition is 0.5cc/min.
The seating material used is Teflon
Operating pressure is 60psig
Differential pressure when closed condition is 70psid
Earlier i were trying with yeild stress value of Teflon for seating load(250psi)168lbf force,however one of articale from emerson defines 40lbf is enough to control 0.5cc/min at 50psig.More the force more the actuation torque required to actuate the ball.
would appreciate your valuable comments
Thanks
John
how much seating force required to control leakage for following requirements.
Allowable leakage when closed condition is 0.5cc/min.
The seating material used is Teflon
Operating pressure is 60psig
Differential pressure when closed condition is 70psid
Earlier i were trying with yeild stress value of Teflon for seating load(250psi)168lbf force,however one of articale from emerson defines 40lbf is enough to control 0.5cc/min at 50psig.More the force more the actuation torque required to actuate the ball.
would appreciate your valuable comments
Thanks
John