I work in a refinery that 'Roasts' ore. I am searching for a material that will cope with 2500 degF - 2700 degF temperature to use as our burner telltale tube. We had used 310 stainless steel but it could not cope with the constant high temperature. Can anyone recommend a material that we can source in a pipe shape that may cope under these conditions. Thanks.