Dear All,
Can anyone tell me the size limitation upto which we can go for seamless pipe or welded pipe.
Specification SA 106, SA 312, SA 790 calls for seamless pipe, but above NPS 12 our supplier is giving welded pipes?
What should be the criteria of acceptance for welded pipes.?
Are there any limitation on the size for the supply of seamless pipes..?
Can small size pipe like NPS 3 to NPS 8 be supplied in welded construction.?