We have several joints that constantly leak. The piping is sch 80 PVC and the liquid is sodium hypochlorite. Has anyone found a thread sealant that works better than others? We cannot glue/weld this joint due to its configuration. Teflon tape is just not doing the trick. Any suggestions?
 
Replies continue below

Recommended for you

You can try Permatex FORM-A-GASKET No. 2 Sealant. It can be used on PVC.

creslinepipe.com/pdf/cresline-west/productapplication&techdata/cwt1.pdf
 
I have not had any luck with Teflon TAPE but have very good luck with a white paste with Teflon. Don't try to use both.

Steve Wagner
 
Note that you should not use pipe dope as it degrades the PVC.
 