Sealing metal before painting

Status
Not open for further replies.

rpeng

Mechanical
Apr 10, 2002
18
I am trying to determine the proper way to seal carbon steel members that are joined by intermittent welds. The steel is cold-rolled ASTM A36 and the final product is epoxy coated with a chemical resistant tank lining (2 coats no primer, 5-6 mils DFT). The final product will be used in an indoor industrial environment (temp 35 - 125 deg F, high moisture, some salt).

I would like to seal the non-welded portion of the intermittent weld before painting while maintaining the appearance and abraision resistance of the product. What procedures/products are recommended? Thank you
 
Replies continue below

Recommended for you

Agree with CoryPad but verify epoxy-sealant compatibility. The epoxy product bulletin should give instructions on surface preparation. In some cases, one prepares polymer concrete by mixing dry (oven baked) silica sand into the resin and then grouts the (preferably sandblasted) cracks.
 