Hello,
in my products I'm using Coprax valves.
after 1-2 months seal is broken - material simply sucks.
Environment is: clear water, max 90C.
So my question is simple
- what kind of rubber/silicone do you suggest? I need to order my own seals - that's the only solution.
Have you got similar problems in past?
in my products I'm using Coprax valves.
after 1-2 months seal is broken - material simply sucks.
Environment is: clear water, max 90C.
So my question is simple

Have you got similar problems in past?