Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

seal material for argon flow

Status
Not open for further replies.

vscid

Nuclear
Joined
Aug 5, 2007
Messages
65
Location
US
If I am flowing Argon inside my solenoid valve, would I be needing Viton seals? Would Buna N work?
Thanks!
 
Buna N should work fine. SBR ("Buna") rubber maybe a little more leak-tight. The only reason to use Viton is if you think your Argon is corrosive, which is unlikely since it's one of the noble gases, and hence very very un-reactive chemically.
 
You should consider the pressures! I assume they are low because if you are operating at high pressures you may experience explosive decompression.

trust this helps.
 