Seal Bearing Sleeve

I have a requirement for a coated or solid sleeve to operate in seawater.
The sleeve will be fitted to a propeller drive shaft with 5 seals running on the outside diameter.

Sleeve duties,
Rotational speed - >600 RPM.
Seal - Shamban Variseal PTFE impregnated with graphite.
The sleeve will rotate submerged in seawater at pressures from 2 - 45 Bar.
When the sleeve is not rotating it will be submerged in seawater at pressures from 2 - 45 Bar, or on the surface subjected to salt spray.

Sleeve Surface Requirements,
Surface Finish - 0.05-0.1 ?m RA Plunge ground.
Material Contact Area Mr - 70%
Determined at a cut depth c=0.25 x RZ relative to the reference line of Cref 5% Mr.
Hardness - 65-70 RC Min

Can anyone advise on an appropriate sleeve material? Information on alternative seals that can operate in this environment would also be appreciated?
 
Can you advise the approximate dimensions of the sleeve?
ie
Outside Diameter
Inside Diameter
Overall length

What experience (if any) have you had with other materials?