Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Sea water analysis

Status
Not open for further replies.

hp22

Chemical
Jul 1, 2006
7
Can anyone let me have typical sea water analysis of sea water of pacific or atlantic sea, preferably in northern hemisphere (values of each salt in mg/l i.e. ppm)?
 
Replies continue below

Recommended for you

Can't find detailed analysis on google....
 
Need urgent help...can anyone spare some time to provide info?
 
Dear HP22
You will find here Sea water Seawater Characteristics in South Atlantic (near from Angola)
Chemical concentration (mg/liter)
Na+ 10178; K+ 279 ; Ca2+ 346; Mg2+ 1132; HCO3- 229;
SO4 2- 2435; Cl- 17166.

Physico-chemical properties
pH 8.1 ;NacL (EQUIVALENT) 31816 mg/l; Specific gravity
@20°C 1.021; Electrical conductivity (20°C) 45.06 mS/cm

source: petrol offshore specifications