All UN, UNS, UNEF, etc are all 60 degree.
UNS means that the thread dimensions are calculated according to ANSI/ASME B1.1 Section 5 and 8, but the designer is supposed to call out the Major Diameter, Pitch Diameter and Minor Diameter since the engagement is a factor in the answer since as the engagement increases, the tolerances loosen. As a result of all of this with the fine threads, minor variations from the required dimensions may have a major impact on strength, and reverse engineering is potentially dangerous. Also plating must be considered properly. With those warnings out of the way the dims are:
Major 1.9062 / 1.8990
Pitch 1.8792 / 1,8764
Minor 1.8494 Min (Max is ref only .18611)
Pitch and minor diameter are reduced as follows:
Engagement Change
1/4" .0006
1/2" .0008
1" .0011
or .001125 x sqrt(engagement (in))