We know what an 8d or 10d common nail is, and we can (or the AF&PA has) tested these at various spacings with various plywoods and OSB’s, etc. In your area there are probably only 8261 different types of screws, so that testing is likely going to have to come from each screw manuf’er. To many over driven nails start to reduce the shear strength of a plywd. shear panels, and this will be true of screw too, which are notoriously over driven.