Can someone tell me what is the difference between the schedule and the Grade for the steel pipes ...

 
Replies continue below

Recommended for you

Schedule is associated with the pipe thickness whereas Grade is normally associated with the material ( For Example 8"nb Schedule 40 - Materials API 5L Grade B)
 