Sep 1, 2023 #1 mechengineer Mechanical Joined Apr 19, 2001 Messages 268 Location SG Hi Experts, Can SB-283 UNS C70620 O20 be used for B16.5 flange? Thabks,
Sep 1, 2023 #2 GDHTX Mechanical Joined Jun 10, 2014 Messages 13 Location US SB-283 C70620 is not a listed material in B16.5-2020 table 1.1-1. ASME B16.24 covers cast copper alloy flanges, so unfortunately SB-283 C70620 is not listed their either. Upvote 0 Downvote
SB-283 C70620 is not a listed material in B16.5-2020 table 1.1-1. ASME B16.24 covers cast copper alloy flanges, so unfortunately SB-283 C70620 is not listed their either.
Sep 3, 2023 Thread starter #3 mechengineer Mechanical Joined Apr 19, 2001 Messages 268 Location SG Thansk @ GDHTX Upvote 0 Downvote