Good evening,
I am checking exchanger tubes in SB-111 061 C44300 under internal and external pressure with ASME VIII div.1.
I have a internal design temperature of 100 °C and external design temperature of 185 °C.
In accordance with ASME IID note G6, the maximum temperature for external pressure not to exceed 175°C, Do we need to reduce external temperature because of this reason or we can do in other way?
Thank you
I am checking exchanger tubes in SB-111 061 C44300 under internal and external pressure with ASME VIII div.1.
I have a internal design temperature of 100 °C and external design temperature of 185 °C.
In accordance with ASME IID note G6, the maximum temperature for external pressure not to exceed 175°C, Do we need to reduce external temperature because of this reason or we can do in other way?
Thank you