Nov 30, 2008 #1 engineermat Mechanical Joined Mar 17, 2008 Messages 47 Location US For SAW, can flux used for PWHT be used for non-PWHT welding? For example, can F7P2 designation be used for Non-PWHT welding?
For SAW, can flux used for PWHT be used for non-PWHT welding? For example, can F7P2 designation be used for Non-PWHT welding?
Dec 1, 2008 #2 weldtek Materials Joined Feb 12, 2005 Messages 897 Location US In some cases you may choose to qualify a WPS with and without PWHT,where the same flux was used. Lincoln certifies certain wire flux combinations with and without PWHT. eg. LA-71 /880M ( P6 A6 ) Upvote 0 Downvote
In some cases you may choose to qualify a WPS with and without PWHT,where the same flux was used. Lincoln certifies certain wire flux combinations with and without PWHT. eg. LA-71 /880M ( P6 A6 )