We have been fabricating 3/16"-3/8" stainless pressure vessels (condensate flash tanks) using FCAW process (dual shield).
But we would like to increase production using SAW process of 304L stainless.
Anyone have any experience in this field/process who could offer insight into what set up to buy, filler metals, flux, etc?
Thanks in advance for any input,
QC Robert
But we would like to increase production using SAW process of 304L stainless.
Anyone have any experience in this field/process who could offer insight into what set up to buy, filler metals, flux, etc?
Thanks in advance for any input,
QC Robert