Saturation vapor pressure of aqueous polyacrylamide solution 1

Status
Not open for further replies.

etsen

Mechanical
Sep 11, 2006
67
What reference book or handbook or website can I find saturation vapor pressure at 10C,20C,30C,40C and compression ratio at room temperature of 5000mg/L aqueous polyacrylamide solution. Would anybody like to tell me that? Thanks a lot.
 
Replies continue below

Recommended for you

Due to the high molecular weight of the polymer, polyacrylamide will have the vapor pressure of a rock. The total vapor pressure will be determined by water.

--Mike--
 