Gentlemen.

I have begun a review of things long forgotten. All to please a customer. As we all strive to do. When we can.

The challenge is to saturate soft ferrite rods with as little power as possible.

The 50% duty coil will cycle, in different applications, at 50 Hertz, 100 Hertz, and 150 Hertz.
 
Replies continue below

Recommended for you

What field strength do you need? Just convert into amp-turns, decide on an operating voltage, and wind a coil.

= = = = = = = = = = = = = = = = = = = =
Plymouth Tube
 
Just test the 50Hz. The others freq. should saturate at larger voltages.

[peace]