Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Sandstone Block Retaining Wall 2

Status
Not open for further replies.

CSEng-Au

Structural
Dec 29, 2019
1
What books or resources would you recommend for the calculation of the sliding friction resistance force of sandstone blocks (between two blocks) in an earth retaining wall?
 
Replies continue below

Recommended for you

If you are doing MSE wall (reinforced earth retaining wall), the linked paper may help.

Link
 
I did a granite one down in Georgia about 45 years back and recollection is fuzzy. I seem to recall that it was about 20' high and 13' wide at the base. There was a masonry 'book' back then that had construction of ashlar walls.

Dik
 
See link from the Foundation Engineering forum; scroll top the post by PEInc

Link

A while back I did a stability analysis of a sandstone stairway. The geotch initially said 0.5 but a lot of the stone was badly weathered so we decided to use 0.4
 