Hello.
Can anyone please tell me how do we sample concrete from ready mixed trucks (say 20 trucks) for making test cubes (say 150mmx150mm).
In my country we use british standard.
 
Why not check the British Standard to find out the procedures?

BA
 
There is not a clear procedure for this. Maybe you could tell me how u do it
 
Concrete testing is to be carried out in accordance with BS 8500-1, Annex B.